PVC Rigid Material Injection Moulding Solutions

Explore PVC rigid material injection moulding for durable precise parts efficient production and reliable industrial performance

PVC Rigid Material Injection Moulding Solutions

Understanding Rigid PVC (UPVC) Material Properties

Rigid PVC (unplasticized polyvinyl chloride) delivers outstanding tensile strength, structural rigidity, flame retardancy, and chemical resistance. In our injection molding operations, working with rigid PVC requires strict discipline because it behaves much differently than commodity polyolefins.

Rigid PVC vs. Flexible Formulations

The primary distinction between rigid and flexible PVC comes down to plasticizers:

Feature Rigid PVC (uPVC) Flexible PVC (Plasticized)
Plasticizer Content None (0%) Moderate to high (up to 50%)
Flexural Modulus High (Rigid, stiff, load-bearing) Low (Elastomeric, bendable)
Thermal Stability Narrow processing window Broader processing window
Common Uses Pressure fittings, valves, conduit Seals, tubing, gaskets

Without plasticizers, rigid PVC retains high dimensional stability and impact resistance, making it an ideal choice for heavy-duty structural parts.

High Melt Viscosity and Shear Flow Behavior

Rigid PVC has high molecular friction and an exceptionally high melt flow viscosity. It exhibits non-Newtonian, shear-thinning behavior:

    • Melt Mobility: The resin does not flow freely under thermal heat alone; it requires applied shear to move through the tool.
    • Frictional Heat: Excessive screw speed or restrictive gates generate localized shear heating. If shear spikes uncontrollably, the melt temperature quickly exceeds safe limits.

Thermal Sensitivity and Hydrochloric Acid (HCl) Risk

Rigid PVC has a notoriously narrow thermal processing window, typically hovering within a tight range before thermal breakdown starts:

    • Degradation Trigger: Prolonged residence time or excessive heat breaks molecular bonds, causing rapid degradation.
    • Corrosive Off-Gassing: Breakdown releases toxic, corrosive hydrochloric acid (HCl) gas.
    • Tool Damage: HCl gas attacks standard mold steels, pit polishing finishes, and strips screw barrels if venting and metallurgy are not configured correctly.

Essential Resin Additives and Modifiers

Pure PVC resin cannot be molded on its own. We process rigid PVC compounds formulated with specific additives to safeguard quality:

    • Thermal Stabilizers: Tin-based or calcium-zinc (Ca-Zn) stabilizers prevent autocatalytic dehydrochlorination during the plasticizing phase.
    • Internal and External Lubricants: Waxes and calcium stearate balance melt homogeneity while preventing the resin from sticking to hot metal surfaces.
    • Impact Modifiers: Acrylics or chlorinated polyethylene (CPE) counteract the natural notch sensitivity of unplasticized PVC, boosting part toughness under mechanical stress.
    • Processing Aids: High-molecular-weight polymers improve melt strength and surface gloss during injection.

Machine Requirements for Rigid PVC Injection Moulding

Rigid PVC injection moulding

Running rigid PVC requires machinery configured specifically to handle aggressive melt flow and prevent material degradation. As a professional injection molding manufacturer and supplier, we do not run unplasticized vinyl on standard general-purpose equipment without dedicated hardware modifications.

Corrosion-Resistant Bimetallic Barrels and Metallurgy

Rigid PVC releases corrosive hydrochloric acid (HCl) vapors if heated past its stable window. Standard nitrided steel components will pit, rust, and fail rapidly under these conditions.

    • Bimetallic barrel lining: We use centrifuge-cast bimetallic cylinders with high nickel-cobalt alloys to resist chemical attack and abrasive fillers.
    • Treated screw surfaces: Screws are chrome-plated or hard-faced with tungsten carbide alloys to prevent chemical pitting and resin sticking.

Screw Geometry and Compression Ratios

Standard plasticizing screws generate excessive shear heat, which burns rigid formulations. A specialized UPVC screw design is mandatory:

    • Low compression ratio: Kept strictly between 1.2:1 and 1.5:1 to avoid extreme shear friction.
    • L/D ratio: Maintained at 18:1 to 22:1, providing sufficient melt homogenization without keeping the heat-sensitive resin in the barrel too long.
    • Zero dead zones: The screw tip features smooth, streamlined smear heads rather than standard three-piece check rings. Any dead corner traps resin, leading to degradation and burned black specks.

Nozzle Types and Stagnation Prevention

Flow stagnation inside the injection unit quickly leads to thermal breakdown.

    • Use open-flow nozzles with direct, short discharge paths.
    • Avoid needle shut-off nozzles, spring-loaded tips, or internal filters that create flow restrictions and dead zones.
    • Equip the nozzle with an independent PID temperature control band to prevent cold slugs without overheating the nozzle seat.

Clamping Force and Machine Tonnage Selection

Because unplasticized PVC has high melt viscosity, it requires substantial injection pressure to fill cavity walls before freezing. Selecting the right machine tonnage ensures part dimensions remain stable without causing flash. When configuring an injection molding machine for sale or shop-floor deployment, factor in higher-than-average cavity pressures.

    • Tonnage rule of thumb: Calculate clamping force using 3.0 to 4.5 tons per square inch (46 to 70 MPa) of the total projected area, including runners.
    • Thick vs. thin walls: Heavy fittings need lower pressure but extended hold, while thin architectural profiles require the upper limit of clamp tonnage to counteract peak cavity pressures during rapid injection stages.
Machine Parameter Standard Plastics Setup Dedicated Rigid PVC Setup
Screw Compression Ratio 2.5:1 – 3.5:1 1.2:1 – 1.5:1 (Ultra-low shear)
Screw / Barrel Material Nitrided Steel Bimetallic Alloy / Chrome Plating
Screw Tip Type Check ring & thrust ring Streamlined smear head (No ring)
Nozzle Design General reverse taper / shut-off Straight open-bore with independent heat
Recommended Clamp Force 2.0 – 3.0 tons/sq. in. 3.0 – 4.5 tons/sq. in.

Mold and Tooling Design Rules for Rigid PVC

Tooling design makes or breaks PVC (rigid material) injection moulding. Rigid PVC won’t forgive lazy mold design: the melt is thick, prone to shear burn, and continually off-gasses acidic vapor under heat. As a professional injection molding manufacturer and supplier, we engineer our molds specifically to withstand aggressive corrosive wear, ease flow restrictions, and prevent trapped volatiles from scorching parts.

For a deeper dive into part geometry and tooling rules, our comprehensive injection mold design engineering book covers essential tolerances and tool-steel selection criteria.

Selecting Corrosion-Resistant Mold Steels

Standard P20 or carbon tool steels degrade rapidly under the acidic conditions generated by rigid PVC processing. When exposed to heat, unplasticized PVC releases trace amounts of hydrochloric acid gas, causing pitting and surface erosion on standard cavity blocks within days.

    • Stainless Mold Steels (S136 / 1.2083): We standardize on ESR (Electro-Slag Remelted) stainless grades like AISI 420, S136, or DIN 1.2083, hardened to 48–52 HRC. These provide superior rust immunity and take a high mirror polish.
    • Hard Chrome Plating: For larger bases or slides where solid stainless inserts drive tooling costs too high, we apply a dense, crack-free hard chrome electroplating layer (minimum 0.03–0.05 mm thick) directly over pre-hardened steels.
    • Corrosion-Proof Core Pins and Inserts: Small cores, ejector pins, and moving lifters must also be made from hardened stainless steel or surface-treated with nickel-based coatings to prevent seizure from corrosive buildup.

Runner Layout, Cold Slug Wells, and High-Flow Gate Configurations

Because rigid PVC has poor melt flow viscosity, restrictive runner geometry generates excessive shear heat that chars the resin.

    • Full-Round Runners: Always use full-round or modified trapezoidal runners. Avoid half-round profiles. Keep runner diameters generous—typically between 6 mm and 10 mm—to allow easy delivery without spikes in injection pressure.
    • Oversized Cold Slug Wells: Place cold slug wells at every runner turn and opposite the main sprue. Any unplasticized cold material that bypasses the wells will plug the gate, cause severe gate blush defects, and weaken weld lines.
    • Gate Selection: Direct sprues, fan gates, edge gates, or heavy film gates work best. Submarine or pin-point tunnel gates should be avoided or widened considerably; their tight constrictions create excessive shear, leading to localized jetting and material breakdown.

Deep Venting Design to Exhaust Corrosive Gases

Trapped air and outgassed volatiles will blister rigid PVC parts, corrode tool steel, and burn component edges. Standard plastic venting of 0.015 mm is often insufficient for rapid clearing of high-viscosity melts.

    • Vent Depth: Run vent depths of 0.03 mm to 0.05 mm on parting lines. Rigid PVC does not flash easily at these depths due to its stiff, viscous nature.
    • Perimeter Venting: Cut wide vent channels (5 mm to 10 mm wide) right up to the cavity land, venting into open atmosphere slots 1.0 mm to 1.5 mm deep around the entire perimeter.
    • Ejector Pin and Core Venting: Flatten ejector pins by 0.02 mm to 0.03 mm on opposing sides or add porous steel inserts in stubborn blind pockets where gas traps occur.
Tooling Parameter Recommended Specification Primary Shop-Floor Benefit
Cavity/Core Steel S136, 1.2083, or Chrome Plating Stops pitting and rust from hydrochloric acid vapor
Runner Profile Full-round, Ø 6.0 mm – 10.0 mm Cuts flow resistance and prevents shear-induced burn
Vent Depth 0.03 mm – 0.05 mm Vents corrosive gas pockets without causing flash
Draft Angle (Internal) 1.5° – 3.0° Prevents part drag marks and vacuum-lock during ejection
Draft Angle (External) 1.0° – 2.0° Ensures clean tool release on textured or polished walls

Draft Angles, Core Pulls, and Cooling Layout

Rigid PVC has a low shrinkage rate (typically between 0.2% and 0.5%), meaning it grips cores tightly as it cools rather than shrinking freely away from deep ribs.

    • Generous Draft Angles: Provide a minimum of 1° to 1.5° on outside walls, and 2° to 3° on deep ribs and internal cores. Tight drafts lead to scuffing, stress whitening, and heavy pin-push marks upon ejection.
    • Mechanical Core Pulls: Use heavy-duty mechanical slides or hydraulic cylinders with positive stops. Keep slide faces well-lubricated with food-grade or high-temp synthetic greases that do not react with halogenated outgassing.
    • Uniform Mold Cooling Channels: PVC transfers heat slowly. Keep water circuits balanced and drilled close to the cavity walls (typically 1.5 to 2 times the drill diameter away from the molding surface). Run mold temperatures strictly between 30°C and 50°C to achieve dimensional stability without inducing internal stresses.

Selecting proper steel and configuring optimized runner networks ensures your tooling lasts through hundreds of thousands of shots without premature surface degradation. For specifications on selecting the right compound grades to match these tooling guidelines, consult our breakdown on raw material rigid PVC injection molding formulations.

Optimal Process Parameters for Rigid PVC Injection Moulding

Dialing in process settings for unplasticized PVC requires tight control. Because rigid PVC has high melt viscosity and extreme shear sensitivity, running loose parameters will burn the resin and ruin parts fast. As a dedicated injection molding manufacturer and supplier, we dial in four core areas on the floor: temperature distribution, injection profiling, packing stages, and screw recovery.

Setting a Narrow Barrel Temperature Profile Zone-by-Zone

Rigid PVC gives you an exceptionally tight thermal processing window. Set temperatures too cold and you risk un-melted pellets and high screw torque; go a few degrees too hot and the material degrades into hydrochloric acid.

Keep a flat or slightly inverted profile toward the rear to prevent premature shear friction, making sure the nozzle zone stays cool enough to eliminate drool without chilling the tip.

Barrel Zone Recommended Setpoint Range Key Purpose
Nozzle 165°C – 175°C (329°F – 347°F) Prevents drool and nozzle freeze-off
Front Zone (Zone 3) 170°C – 180°C (338°F – 356°F) Final melt homogenization without scorching
Middle Zone (Zone 2) 160°C – 170°C (320°F – 338°F) Progressive plasticizing and air release
Rear Zone (Zone 1) 150°C – 160°C (302°F – 320°F) Feed stability; limits early agglomeration

Multi-Stage Injection Speed to Limit Shear Heat

Friction generates heat rapidly when forcing stiff melt through small gates. Never shoot rigid PVC at a single, flat-out injection speed.

    • Slow start: Break through the gate smoothly to stop jetting and gate blush.
    • Moderate main fill: Accelerate through the thick body sections to fill 90% to 95% of the cavity volume.
    • Deceleration before transfer: Drop injection speed right before the switchover to protect thin ribs and prevent flash or burn marks at the end of fill.

Controlling these dynamic cycles is essential when evaluating part quality and production efficiency against tooling and injection competition costs over high-volume runs.

Holding Pressure Duration and Packing Levels

Rigid PVC cools from the outside in with noticeable volumetric shrinkage. Because of its thick cross-sections in parts like pipe fittings, proper holding pressure prevents sink marks and vacuum voids without over-packing the gate area.

    • Packing Pressure: Set holding pressure at roughly 50% to 70% of peak injection pressure. High hold pressures cause high molded-in stress, resulting in brittle parts that crack under load.
    • Holding Time: Maintain pressure just until the gate freezes completely. Use a precise part-weighing study to confirm gate seal time; packing after gate seal only stresses the sprue and wastes cycle time.

Screw Back Pressure and Low RPM Settings

Plasticizing UPVC requires patience. High rotational speeds quickly generate runaway frictional heat inside the barrel flutes.

    • Screw Speed (RPM): Keep screw recovery slow—typically 25 to 45 RPM. Running the screw too fast shears the polymer chains and turns stabilized compound yellow.
    • Back Pressure: Run minimal back pressure, generally between 3 and 8 bar (45 to 115 psi). This provides just enough resistance to purge entrapped air out of the melt stream without generating excessive mechanical shear.
    • Decompression (Suck-Back): Use a minimal stroke (2 to 5 mm) at low speed. Over-decompression pulls atmospheric oxygen into the nozzle tip, oxidizing remaining PVC and causing black specks on the subsequent shot.

Troubleshooting Rigid PVC Injection Moulding Defects

Rigid PVC does not forgive sloppy processing. Because the resin is extremely shear-sensitive and has a razor-thin thermal processing window, running it requires fast diagnosis of part flaws on the plant floor. We balance these tight material limits against the broader advantage and disadvantage of injection moulding to optimize tool parameters and eliminate scrap early.

Discoloration, Yellowing, and Burned Black Specks

Thermal degradation is the main trigger when unplasticized PVC turns yellow, brown, or spits out black carbon specks.

    • Drop the barrel temperature: Lower nozzle and front zone temperatures by 5°C to 10°C increments to keep the melt below the degradation threshold.
    • Lower screw RPM: Excessive screw rotation generates severe shear heat. Drop screw speed down to 25–40 RPM.
    • Reduce residence time: Ensure the machine shot size utilizes 40% to 70% of the total barrel capacity. Sitting too long in a heated barrel causes rapid thermal breakdown.
    • Inspect screw geometry: Eliminate dead zones on the screw tip or nozzle adapter where stagnant material can bake and char.

Short Shots and High-Pressure Flow Lines

Rigid PVC features exceptionally high melt viscosity. If the melt front cools too fast or encounters flow resistance, incomplete fills and dull flow bands emerge.

    • Enlarge runner and gate cross-sections: Restricted runners strangle the flow. Open runners and use direct sprue, tab, or fan gates to feed thick sections.
    • Step up mold temperature: Cold mold walls freeze the skin too early. Raise mold cooling water to 30°C–50°C to allow smooth cavity filling without packing pressure spikes.
    • Clean and deepen tool venting: Trapped air blocks melt advancement. Ensure parting-line vents are clean and ground to a depth of 0.03 mm to 0.05 mm.
    • Utilize staged injection velocity: Start slow through the gate, ramp up fill speed to maintain melt front momentum, and slow down just before transfer.

Jetting, Gate Blush, and Weld Line Weakness

When unplasticized PVC shoots through a narrow gate at high velocity, it snakes into the cavity without adhering to walls, causing visible snake-skin jetting, halo gate blush, and weak structural seams.

    • Rethink gate location and type: Direct the gate toward a cavity wall, core pin, or rib to break up the incoming stream. Sub-gates and overlap gates minimize blush significantly better than pin gates.
    • Slow down initial injection speed: Use multi-stage injection profiles. Set velocity low during gate transition, then speed up once the cavity begins expanding.
    • Boost weld line fusion: If weld lines split or look prominent, increase injection packing pressure slightly and place overflow tabs or vents right at the knit line interface.

Silver Streaks and Moisture-Induced Splay

Silver splay streaks across the part surface usually point to surface moisture on fillers, volatilized additives, or air trapped during screw recovery.

    • Pre-dry resin: While rigid PVC base resin absorbs minimal water, impact modifiers and calcium carbonate fillers pull in surface moisture. Dry material at 65°C–70°C for 2 to 3 hours.
    • Cut back screw decompression (suck-back): Excessive suck-back pulls ambient air through the nozzle tip into the melt stream, creating parabolic silver streaks during the shot.
    • Raise back pressure: Set moderate back pressure (0.5 to 1.5 MPa) during dosing to compact the melt and evacuate trapped air back through the hopper throat.

Safety Protocols, Purging, and Equipment Maintenance for Rigid PVC

Running rigid PVC requires strict plant floor discipline. When processing unplasticized polyvinyl chloride, excessive heat turns melt into hydrochloric acid (HCl) gas fast. As we scale up production and continuously expand our moulding production capacity, we stick to clear safety, purging, and preventative tooling protocols on every shift.

Managing Acid Gas Emissions and Ventilation

Overheated PVC releases pungent, acidic white smoke that irritates the eyes, throat, and lungs, while corroding nearby machinery.

    • Dedicated Exhaust Hoods: Position localized exhaust extraction hoods directly above the machine barrel and mold platen area to capture off-gassing immediately.
    • Worker Safety Gear: Operators must keep acid-gas respirators, safety goggles, and thermal gloves nearby at the press.
    • Airflow Management: Maintain active cross-ventilation across the shop floor to prevent fumes from accumulating near overhead cranes and controllers.

Safe Purging Procedures: Start-Up and Shutdown

Leaving rigid PVC sitting hot in the barrel during breaks guarantees black specks, degradation, and screw pitting. Purge properly every single time.

    • Start-Up: Never bring a cold machine up to temperature with rigid PVC packed inside the barrel. Preheat using a high-viscosity, high-stability resin like fractional melt HDPE or dedicated commercial purge compounds until processing temperatures equalize.
    • Transitioning to PVC: Run purging material until it shoots completely clear, then feed rigid PVC pellets and push out the purge resin at low screw RPM.
    • Normal Shutdown: Stop the PVC feed and pump the barrel empty. Immediately introduce HDPE or specialized chemical purging compounds to scrub every trace of PVC off the screw flights and barrel walls before lowering heat zones.

Emergency Shutdown When Material Burns

If a cycle interrupts or you notice heavy yellowing, black specks, or visible acid smoke, act within seconds:

    • Kill the Barrel Heaters: Turn off all zone heats instantly.
    • Back Out the Injection Unit: Retract the nozzle carriage entirely away from the sprue bushing.
    • Purge Immediately: Feed low-melt HDPE or purging compound through the hopper and purge continuously at low speed until the black, degraded PVC clears out.
    • Air Out the Station: Turn ventilation hoods to maximum draw and clear non-essential staff from the immediate bay area.

Preventative Tool Maintenance and Rust Defense

Acid byproduct from rigid PVC attacks non-plated tooling steels quickly if left untreated.

Maintenance Step Action Protocol Frequency
Venting Scrub Clean vent slots with brass tools and mild neutralizing solvent Every 4 to 8 hours
Cavity Wipe-Down Wipe parting lines and cavities with alkaline cleaner to neutralize acid residues Every shift change
Short-Term Protection Spray an acid-neutralizing rust inhibitor across the open tool face Any shutdown over 1 hour
Long-Term Storage Deep-clean cavities, apply heavy anti-corrosion grease, and seal the mold closed Tool pull / job completion

Industrial Applications of Rigid PVC Injection Molded Components

Rigid PVC provides exceptional tensile stiffness, weatherability, and flame resistance at a fraction of the cost of higher-end engineering thermoplastics. While flexible components rely on soft PVC injection molding for gaskets and seals, rigid unplasticized formulations take the structural load in harsh chemical and mechanical environments.

We are a professional injection molding manufacturer and supplier, regularly running high-precision PVC (rigid material) injection moulding for parts that demand exact tolerances and zero structural compromise.

    • Plumbing & Pressure Pipe Fittings: High-volume production of elbows, tees, couplings, unions, and bushings engineered to endure sustained water pressure and resist scaling in drainage, waste, and municipal systems.
    • Electrical Enclosures & Conduit Hardware: Non-conductive electrical junction boxes, raceway fittings, switch faceplates, and underground conduit elbows delivering natural UL94 V-0 flame-retardant performance without heavy additive costs.
    • Chemical-Resistant Fluid Handling: Rugged ball valve bodies, check valves, flow meters, filter housings, and industrial pump components designed to safely handle aggressive acids, bases, and corrosive effluent streams.
    • Building Products & Exterior Fasteners: UV-stabilized construction clips, structural siding fasteners, window profile end caps, and outdoor drain channels built for long-term weather resistance without warping or UV embrittlement.

Frequently Asked Questions About Rigid PVC Injection Moulding

Running unplasticized vinyl on the shop floor leaves zero margin for guesswork. As a dedicated team managing high-volume tooling and parts, we get asked these exact technical questions when setting up PVC (rigid material) injection moulding programs.

What is the ideal processing temperature window for rigid PVC?

The workable melt temperature window for rigid PVC is remarkably tight, typically sitting strictly between 330°F and 395°F (165°C to 200°C).

    • Rear barrel zones: 300°F – 320°F (150°C – 160°C) to start gentle conveying without packing the feed throat.
    • Middle zones: 330°F – 355°F (165°C – 180°C) for controlled plastification.
    • Front and nozzle zones: 360°F – 385°F (182°C – 196°C) to deliver melt to the tool without shearing the polymer chains.

If your melt drops below 330°F, you face extreme melt viscosity, severe screw motor load, and immediate short shots. Push it past 400°F (205°C), and the material will char within minutes.

Why does rigid PVC degrade and release corrosive acid so quickly?

Rigid PVC lacks the plasticizers that lower melt friction in flexible grades, meaning it generates intense mechanical shear heat. The chlorine atoms bound to the polymer backbone are fundamentally sensitive to excess heat and residence time.

Once thermal limits are exceeded, an autocatalytic dehydrochlorination reaction starts:

    • Chain degradation: The chemical bonds snap, liberating volatile hydrochloric acid (HCl) gas.
    • Corrosive attack: Escaping HCl vapor reacts with ambient air moisture, attacking standard tool steels, barrel walls, and tie bars.
    • Pitting and destruction: Without specialized stabilizer packages and corrosion-resistant alloys, the acid permanently pits the cavities and degrades your machinery.

Can regrind or scrap rigid PVC be blended back into production?

Yes, but it requires tight discipline. For standard industrial and plumbing fittings, clean, unburned regrind can be blended at 5% to 15% without compromising structural tensile properties.

Never reintroduce material that has undergone even minor thermal discoloration or yellowing, as its chemical stabilizer package has already been depleted. For thin-walled electrical housings, tight-tolerance components, or parts requiring certified weatherability, we strictly run 100% virgin resin to guarantee structural integrity and uniform shrinkage rates.

How do you stop gate blush and jetting marks on thick-walled UPVC parts?

Gate blush and snake-like jetting marks happen when high-viscosity melt shoots through a narrow orifice into an open cavity at excessive speed. To eliminate these flaws in thick-walled sections, we utilize specific tooling and process corrections:

    • Switch to submarine, fan, or edge gates with generous cross-sections: Direct the flow against a cavity wall or core pin immediately upon entering the tool to force a steady, expanding fountain flow.
    • Use profiled, multi-stage injection velocities: Inject at a very low speed (5% to 15%) until the melt clears the gate entry, then ramp up fill speed once the flow front stabilizes.
    • Optimize mold temperatures: Keep cavity temperatures warm—between 85°F and 130°F (30°C to 55°C)—so the skin layer does not freeze prematurely and tear under incoming melt pressure.

Mastering these design and velocity trade-offs is a core focus across our dedicated PVC injection moulding operations to keep scrap rates near zero.

What is the best material to purge rigid PVC out of the barrel?

Never let rigid PVC sit stagnant in a hot screw during breaks, shift changes, or shutdowns.

    • High-Density Polyethylene (HDPE): A fractional melt index HDPE is the most reliable, cost-effective mechanical purge resin. It scrubs the screw flights clean, pushes out residual vinyl, and tolerates heat without degrading.
    • General-Purpose Polystyrene (GPPS): Excellent for a quick physical clear-out when changing over to other high-temperature engineering resins.
    • Commercial chemical purge compounds: Specially formulated chemical purging compounds designed for vinyl strip residual material and neutralize corrosive chloride ions effectively.

Always flush the barrel with HDPE until the purge stream runs pure white and smooth before dropping barrel heats or turning off the machine.

en_USEnglish